Lecture 11 on Topics 8 and 9: Mechanical Properties; Glass Strengthening
MIT OpenCourseWare
Griffith cracks in glass 0:00
Glass breaks far below its theoretical strength because tiny cracks act as defects. A bulk crack is described with a length of 2a, while a surface crack is treated as a crack of length a. The applied far-field stress is written as sigma infinity, but the stress rises sharply at the crack tip. That concentration is much larger than the atomic spacing a0, so the crack tip becomes the weak point and the crack grows. Using this idea, the fracture strength drops with crack length. For silica glass, a measured strength of about 110 megapascals corresponds to a crack about 5 microns long, which is enough to explain the large gap between theory and practice.
Metallic Glass Toughness 18:01
Bulk metallic glass breaks differently from oxide glass. As a crack opens, the material can deform in shear instead of simply separating. That local plastic flow absorbs energy and raises fracture toughness. An empirical rule uses the shear modulus divided by the bulk modulus: below a threshold, the glass tends to be plastic; above it, brittle. This is why some bulk metallic glasses sit in the high-strength, high-toughness corner of the strength-toughness plot.
Cracks And Fractography 22:01
In oxide glass, cracks usually start at surface defects and run very fast, about one third to one half the speed of sound in glass. Glass is still not perfectly brittle, because it can densify a little as it cracks. That is why strengthening methods focus on surface flaws. Fractography then uses the broken surface to tell you where failure began and how it spread. The mirror, mist, and hackle regions, along with Wallner lines, help you read that history.
Fracture clues and fatigue 34:30
Fractured glass can be read like a record of the break. Near the impact point, you see the mirror region, then mist and hackle, and farther out Wallner lines, which come from elastic waves meeting the crack tip. The mirror zone is only a few hundred microns wide and gets smaller when the applied stress is higher, while mist and hackle sit in the millimeter range. Wallner line spacing depends on the difference between elastic wave speed and crack speed, so thinner glass or faster cracks change the pattern. These markings apply to non-tempered glass. Tempered glass breaks differently because surface compression pushes the main defect into the interior, leaving center mist and hackle, symmetric Wallner lines outside, and horizontal surface marks. Glass can also fail later under loads below the fracture stress. That static fatigue comes from stress corrosion: water vapor condenses in a surface crack and slowly attacks the glass network.
Fracture testing and statistics 51:01
Glass often fails from surface cracks, and even tiny amounts of water can feed subcritical crack growth. Because of that, fracture toughness is measured with standard ASTM methods or with simpler indentation tests. In indentation, a hard tip such as a Vickers pyramid is pressed into the glass, and cracks usually appear on unloading, when elastic recovery meets plastic damage. The crack pattern then gives an estimate of toughness. These measurements are statistical, because the longest defect often controls failure. The Weibull distribution describes the spread. A larger Weibull modulus means a tighter, more consistent strength, and a bimodal curve can reveal two defect populations in the same sample set.
Ways to strengthen glass 1:08:02
Three routes are given for stronger glass: lower crack driving force, remove surface defects, or keep cracks closed with surface compressive stress. Crystallization, polishing, etching, coatings, and tempering all fit these aims, and glass ceramics can gain density and stress benefits, though transparency may be lost.
AI-generated summary. It can be wrong or incomplete - check anything that matters against the original.